请登录后使用此功能。 您可以使用此功能将商品添加到您的收藏列表。
关闭
您已经添加该商品到您的收藏列表。 查看我的收藏
关闭
从您收藏列表中删除此商品。
关闭
请登录后使用此功能。 您可以使用此功能将公司添加到您的收藏夹列表。
关闭
这家公司已成功添加。 查看我的收藏
关闭
这家公司已从你的收藏夹列表中删除。
关闭
请登录后使用此功能。 您可以使用此功能将公司添加到您的询问车。
关闭
这家公司已被添加到您的询问车。
关闭
这家公司已从询价车中删除。
关闭
该商品已被添加到您的询问车。
关闭
该商品已经从您的询价车中删除。
关闭
商品/公司已达到添加至询价车的数量。
关闭
ABV Global Holdings Sdn. Bhd.
ABV Global Holdings Sdn. Bhd. 201401041142 (1117296-H)
SSM
商业性质:

提供者 分销商

AMILAN!" Nylon Resin About heat-resistant nylon resins CM1026 and CM3006 - Injection-molding - ABV Global Holdings Sdn. Bhd.

AMILAN!" Nylon Resin About heat-resistant nylon resins CM1026 and CM3006 - Injection-molding

07-Jun-2024

Molding conditions

Both CM1026 and CM3006 can be molded using the same conditions as standard grades.
In terms of resin temperature, use a 230-260°C molding temperature for CM1026 and 260-290°C for CM3006. A mold temperature of about 60-80°C is appropriate for both CM1026 and CM3006.
Regarding flowability, spiral flow-length tests show about L/T200 works well for both CM1026 and CM3006.
If master color pellets will be mixed into the pellets to add colors such as black, use a screw type injection-molding machine.
For more detailed data on injection molding, refer to Toray’s injection-molding guide.

Mold design

Mold shrinkage is influenced by a complex combination of factors—product shape and thickness, molding temperature, mold temperature and pressure, among others. See Figure 32 for an example using CM3006. The data was generated using a flat plate-shaped product. Cylindrical products have a mold shrinkage rate that is about 70% that of flat plate-shaped products.
A draft angle of about 1° to 1.5° is appropriate for the inside surface of a cylindrical product, where a larger draft angle is required, in particular.
A mold temperature within the range of 60-80°C is appropriate, and it is important to keep the temperature as uniform as possible.

\"Figure \"Figure

Figure 32: Molding conditions and mold shrinkage (%)

Pellet water absorption

Nylon is water-absorbent. To avoid bubbles, silver streaking and other quality issues caused by water absorption, dry the pellets to about 0.2% water content or less before molding. Coming off the manufacturing line, the nylon pellets have been dried to a level no higher than 0.1% water content, so there is no need to dry the pellets if used immediately after opening. However, leaving the pellets inside the hopper for extended periods of time will allow gradual water absorption that could lead to quality issues.
To assess the water absorption speed of CM3006, change in weight under various humidity conditions was measured. See Figure 33 for the test results. Assuming an allowable water content of no higher than 0.2%, the pellets can be left out in the open for no more than 20 hours at 40% RH and about one hour at 80% RH.

\"Figure

Figure 33 Nylon 66 pellets speed of water absorption

Material: nylon 66 (CM3001N and CM3006)
Pellet shape: 3.0 × 3.0 × 3.0mm
Temperature: 23±1°C
Humidity: 40-80±3%RH

总办事处

ABV Global Holdings Sdn. Bhd. 201401041142 (1117296-H)
109, Jalan Iks Juru, Taman Perindustrian Ringan Juru, 14100 Simpang Ampat, Pulau Pinang, Malaysia.

电话:

邮件:
网址: https://www.abvglobalholdings.com
网址: https://abvglobalholdings.newpages.com.my/
网址: https://abvglobalholdings.onesync.my/

游览 : 首页 - 分类 - 公司 - 地区 - 标签 - 商品 - 消息与促销 - 工作征聘 - 手机版 - 谷歌 - 搜索引擎优化结果

NEWPAGES

  • US 8031
  • BR 2075
  • SG 1350
  • AU 1327
  • CA 1239
  • TH 1204
  • JP 1148
  • MY 868
人 在线
Seni Jaya Logo
Brochure
Download
Our PackageContact Us