CRN-MULTILAYER
The coating for protection against corrosion and oxidation
CrN coatings are the best choice for applications where resistance to abrasion, corrosion and oxidation is required. The high hardness and very low brittleness allow thicker CrN coatings with very good adhesion to the substrate.
|
Hardness |
2,000 ± 200 HV |
|
Max. temperature of operation |
600 °C |
|
Coeff. of friction against steel |
0.3 – 0.4 |
|
Coating thickness |
2-6 µm |
|
Colour |
Silver grey |
COATING ADVANTAGES
• High hardness and adhesive strength• Very good chemical resistance
• Low friction coefficient against steel
• High temperature resistance in air
• Low residual stress
• Significantly improved corrosion resistance due to multi-layer structure (e.g. plastic injection: treatment of PVC or flame protection)
APPLICATIONS
Plastic injection
•Tools which are subject to corrosive and abrasive wear, e.g. through aggressive and hard filling materials•Significantly reduced formation of deposits
Forming
•Drawing, stamping, pressing and forming tools for the working of non-ferrous metals, especially Ti and Cu alloysMagnesium die casting
•Mould inserts and cores which are subjected to corrosive stress•Significantly improved demoulding (in connection with polishing)




BR 27271
VN 13660
US 6659
AR 4979
CN 3549
MX 3545
IQ 2009
CO 1875